Friction and Mould Wear in Brick Presses: Causes, Effects and 8 Proven Solutions

Why friction in brick moulds reaches 20–100 % of pressing force, how it wears moulds and presses, and eight ways to reduce it, from coatings to degassing.

Brick press mold and tooling — Friction Challenges in Brick Molds: Causes and Solutions
Key points
  • Friction between the mix and the mould ('locking') can reach 20–30 % of pressing force or more.
  • Ejection force: up to 100 % of pressing force for salt, up to 50 % for clay, 20–30 % for limestone.
  • Friction wears moulds into a 'spindle' shape, raises energy use and causes cracks on ejection.
  • Chrome, metal-ceramic or ceramic surfaces, mould heating to 60–80 °C and degassing cycles all help.

In high-pressure brick moulding, one persistent challenge is friction between the raw material and the mould surfaces — the punches (puncheons), the matrix and the core formers. This effect, often called “locking” or “sticking”, increases mould wear, wastes energy and can compromise product quality. This article explains why friction occurs, which factors drive it and which practical solutions manufacturers can adopt.

up to 100 %ejection force, salt
up to 50 %ejection force, clay
20–30 %ejection force, limestone
60–80 °Cmould heating for clay

Understanding the problem: friction and locking

When raw materials are pressed at high pressure, the compacted product pushes outwards against the mould walls. This lateral pressure, combined with adhesion between the material and the steel, creates friction that must be overcome every time the product is ejected. The frictional forces can reach 20–30 % of the pressing force or more, and in some cases may equal it:

Raw materialTypical ejection force (share of pressing force)Adhesion to mould
SaltUp to 100 % — can equal the pressing forceVery high
ClayUp to 50 %High
Limestone-based mixes20–30 %Lower

The locking effect is particularly pronounced in materials such as clay and salt, which adhere strongly to mould surfaces.

Why friction grows with product height

A compacted powder does not behave like a liquid. Part of the vertical pressing force is turned into sideways pressure on the mould walls, and the friction on those walls in turn absorbs part of the force on its way down through the material. The taller the product, the more wall area there is and the more force is lost before it reaches the bottom. Two consequences follow:

  1. Density gradients. The part of the brick nearest the moving punch is compacted more than the far end, unless the press compacts from both sides.
  2. High ejection loads. After pressing, the elastic spring-back of the compacted material keeps it pressed against the walls, so the press must push hard to eject it — the “locking” effect.

This is why product geometry, mould surface and press design must be considered together.

How friction affects production

  • Increased mould wear. Friction concentrates stress in specific areas, so the mould wears unevenly and gradually takes on a “spindle” (barrel) shape. Core formers and other components may deform under prolonged stress.
  • Higher energy consumption. The extra force needed to eject the product increases energy demand on every cycle.
  • Compromised product quality. Excessive friction can cause cracks or surface defects during ejection.
  • Reduced press durability. Prolonged high friction strains the press structure and shortens its service life.

A worn, spindle-shaped mould also produces bricks that are slightly wider in the middle than at the ends, which matters for precision products and for interlocking or robot-laid bricks.

Factors that influence friction in brick moulds

1. Contact surface area

Larger contact areas create more friction. Tall bricks, and highly porous (thin-walled hollow) bricks with many core formers, are particularly susceptible.

2. Raw material properties

Salt shows extremely high ejection forces (up to 100 % of pressing pressure), clay moderate ones (up to 50 %) and limestone lower ones (20–30 %). Particle size, composition and moisture further influence friction.

3. Raw material moisture

Dry materials tend to stick more but press more efficiently. Moist materials reduce friction but may compromise the pressing process. The right moisture is therefore a balance.

4. Mould material

Chrome, metal-ceramics and ceramics reduce friction better than standard steel.

5. Temperature of mould and raw material

Heating the mould to 60–80 °C can reduce adhesion for certain raw materials, such as clay.

Eight solutions to reduce friction

  1. Optimise product dimensions. Reducing the product height minimises the contact area and therefore friction.
  2. Adjust raw material moisture. Find the optimum moisture level that improves flow and reduces sticking while keeping the product sound.
  3. Heat the mould. Preheating reduces sticking for materials such as clay and salt.
  4. Modify raw material properties. Additives can change the flow characteristics of the mix, making it easier to press and eject.
  5. Use advanced mould materials. Chrome plating, metal-ceramics and ceramics reduce adhesion and improve mould durability.
  6. Optimise mould geometry. Adjusting the angles of the matrix walls and core formers makes ejection smoother.
  7. Improve surface coatings. Chrome plating or ceramic coatings reduce friction and increase wear resistance.
  8. Use advanced degassing. Pressure-holding cycles and degassing programmes release trapped air during pressing, reducing internal stress and friction.
Longer mould life: wear-resistant materials are one of the most effective levers. Read how we use tungsten carbide to prolong press mould life.

Benefits of reducing friction

  • Lower pressing pressure: less friction means less force is lost, so the same density is reached with lower compaction force.
  • Longer mould life: less wear reduces replacement costs.
  • Better product quality: fewer cracks and more consistent dimensions.
  • Energy savings: less power for both pressing and ejection.
  • Higher reliability: smoother operation and fewer breakdowns.

How TITAN designs presses and moulds against friction

Friction in brick moulds needs careful attention during both design and production. TITAN designs its brick presses with these challenges in mind — from advanced mould materials to optimised press designs — so the equipment runs smoothly and efficiently even under the most demanding conditions.

Struggling with sticking, cracked products or fast mould wear? Contact us with details of your raw material, or explore our press moulds and custom hydraulic presses.

Frequently asked questions

How large can friction forces in a brick mould be?

Typically 20–30 % of the pressing force or more. For salt the ejection force can equal the pressing force, for clay it can reach 50 %, and for limestone it is usually 20–30 %.

Does heating the mould reduce sticking?

Yes, for certain raw materials such as clay. Heating the mould to 60–80 °C can reduce adhesion.

Which mould materials reduce friction?

Chrome plating, metal-ceramics and ceramics perform better than standard steel and also improve wear resistance.

How does degassing help?

Pressure-holding cycles and degassing programmes release trapped air during pressing, which reduces internal stress and friction.